VDM Metals - Model 718 -Superalloys
Super alloys like VDM Alloy 718 are nickel or cobalt based alloys that are, on the one hand, used around significantly heightened temperatures, but on the other hand also in extremely corrosive environments. The driving force in the development of these materials were the increasingly higher requirements of the aviation industry, caused by higher temperatures in turbines. Further areas of application for semi-finished products of Ni-based superalloys are chemical plants with extreme requirements for corrosion resistance as well as nuclear power plants.