The depolymerization of plastics and rubber is the basis of the waste-to-diesel process. The plastics and rubbers are gradually heated to temperatures of 400 to 450 ° C. During the depolymerization long carbon chains such as plastics and rubbers set into shorter chains, typically a chain length C8 to C20.Generally something is considered gasification if the temperature exceeds 800 ° C. Pyrolysis is the process that occurs under anearobic conditions at 500 to 800 º C. At temperatures of 300 to 400 ° C, we speak of torrefaction, while pyrolysis of plastics at temperatures up to 400 to 450 ° C is called depolymerization.
-